Renewable Energy

Emulsion layer limits screen-printing damage in copper-plated HJT cells

A 4.7% emulsion coverage ratio reduced minority-carrier lifetime degradation while maintaining acceptable photoresist uniformity, researchers report.

Maya LindqvistNovember 15, 20265 min read2 views

A close-up conceptual view shows a fine screen mesh above a solar-cell wafer, with a thin emulsion layer separating the two during printing.

Researchers in China have investigated how screen printing degrades copper-plated silicon heterojunction (HJT) solar cells and proposed a modification to the printing screen that reduces the damage. The work focuses on the photoresist-coating step used in copper metallization, where the screen comes into direct contact with the wafer across most of its area.

Screen printing is widely used to form metal contacts on solar cells, but mechanical pressure and thermal treatment can harm HJT cells’ sensitive passivating contacts. The resulting recombination losses can lower open-circuit voltage and fill factor. The team said previous production data showed conversion efficiency falling from 26.2% to 25.7% over 15,000 consecutive printing cycles, while short-circuit current density and electrical resistance remained largely unchanged.

Measurements also showed that minority-carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles. Using three-dimensional confocal microscopy, the researchers identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles flattened or wore, their contact area with the wafer increased, raising mechanical stress on the passivation layers beneath.

Scanning electron microscopy found no visible surface scratches, but photoluminescence measurements indicated greater recombination. The researchers linked this to damage at the amorphous silicon/crystalline silicon interface. They said the photoresist printing process differs from conventional silver-paste printing: silver screens have openings covering only 2–5% of the area and an emulsion layer prevents direct mesh-wafer contact, whereas full-area photoresist coating typically uses a screen without emulsion coverage. That design allows uniform resist deposition but brings the mesh into broad contact with the wafer on every cycle.

To reduce that contact, the team added an emulsion buffer layer to the screen. The team evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6%. Higher coverage protected the wafer but interfered with photoresist distribution, creating a trade-off between mechanical protection and coating uniformity. A coverage ratio of 4.7% gave the best balance, limiting minority-carrier lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good coating uniformity.

The researchers attributed the improvement to the emulsion layer preventing direct contact between the screen mesh and the wafer, which reduced cumulative mechanical damage to the passivating layers. Corresponding author Lang Zhou said the results show that a relatively simple screen-design change can substantially mitigate printing-induced degradation and offer a practical route to more reliable manufacturing of copper-plated HJT cells.

The findings were published in Solar Energy. The study adds to broader efforts to replace silver in HJT metallization with copper. In April 2026, researchers at Nankai University reported a silver-free HJT cell with 25.2% efficiency using plasma-induced interface engineering and copper electroplating, addressing adhesion, contact resistance and stability at the ITO interface. Separately, researchers at Forschungszentrum Jülich achieved 23.08% efficiency in a fully copper-metallized HJT cell, with a relatively small penalty versus a silver-metallized counterpart; cells using silver-copper paste on the front and silver contacts on the rear reached 23.95%.